Universal Wire Works ER320 Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER320 Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition of copper and columbium to the alloy content provides resistance to intergranular corrosion. Alloy 320 is designed to weld base metals of similar compositions for applications where resistance to severe corrosion involving a wide range of chemicals including sulfuric and sulfurous acids and their salts is required. Alloy 320 can be used for welding wrought and cast alloys of similar composition without postweld heat treatment.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Chromium, Cr 20 %
20 %
Copper, Cu 3.5 %
3.5 %
Iron, Fe 36.5 %
36.5 %
As Remainder
Molybdenum, Mo 2.5 %
2.5 %
Nickel, Ni 34 %
34 %
Niobium, Nb (Columbium, Cb) 3.5 %
3.5 %