Material Notes:
Made for non-woven textiles applications. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527
Elongation at Break >= 200 %
>= 200 %
ISO 527
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ISO 75
Vicat Softening Point 154 °C
309 °F
ISO 306