Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct ASTM E2336 System

Category Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name FyreWrap®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct ASTM E2336 System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unifrax's FyreWrap ™ 1.5 Duct Insulation is a two-layer flexible enclosure for one- and two-hour rated commercial kitchen grease ducts and hazardous exhaust ducts including chemical fume ducts. FyreWrap 1.5 Duct Insulation is tested per ASTM E-2336 and is acceptable as an alternate to a traditional fire-rated shaft. Installed as a two-layer system, FyreWrap 1.5 complies with AC101 and the 2006 Edition of the International Mechanical Code (IMC). FyreWrap 1.5 Duct Insulation offers the following product feature:Complies with 2006 IMC and UMCTested per ASTM E-2336Two-layer system; inner layer utilizes butt jointHigh-temperature, biosoluble insulationZero clearance to combustibles, at any location2-hour fire endurance ratingAlternate to shaft enclosureGREENGUARD listed for Microbial ResistanceProduct ComponentsCore Material: FyreWrap 1.5 incorporates Insulfrax Thermal Insulation as its core material. Insulfrax is a high-temperature insulation made from a calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket product form.Encapsulating Material: The core insulation blanket is completely encapsulated in an aluminum foil fiberglass reinforced scrim covering. This scrim provides additional handling strength as well as protection from moiture absorption and tearingInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.0961 g/cc
0.00347 lb/in³
Nominal
Thickness 38100 microns
1500 mil
Thermal Properties Metric English Comments
Insulation R Value 6.19
6.19
ASTM C518
Descriptive Properties Value Comments
ASTM C136 Non-combustibility Pass