Trimay® Wear Plate TWP56 Chromium-based Flux Cored Weld Wire & Electrode

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Trimay® Wear Plate Ltd
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trimay® Wear Plate TWP56 Chromium-based Flux Cored Weld Wire & Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: TWP56 is a chromium-based flux cored wire electrode used to protect equipment and parts from moderate wear and impact. TWP56 has wide welding parameters, allowing for easy installation, and its compatible composition allows it to be applied on a wide array of materials.Key Performance Characteristics: Moderate abrasion and impact resistance, Compatible composition, Uniform carbide distribution throughout weld deposit, Ease of use (wide voltage and amperage welding parameters)Applications: TWP56 can be overlain on carbon steel, manganese base materials and mild or alloy steels. The maximum recommended deposit thickness of TWP56 is 2 - 3 layers, or 1/4” (6.35mm). TWP56 is primarily used to cover exposed bolts and seams from installation of T138 wear plate and parts, however, TWP56 wire and electrodes are also welded to parts and equipment which require protection only on one or two concentrated wear areas.Information provided by Trimay®
Mechanical Properties Metric English Comments
Hardness, Rockwell C 52 - 58
52 - 58
Wire
57 - 60
57 - 60
Electrodes
Component Elements Properties Metric English Comments
Carbon, C <= 5.0 %
<= 5.0 %
Chromium, Cr <= 27 %
<= 27 %
Iron, Fe >= 65 %
>= 65 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Silicon, Si <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Available Sizes: Electrode 3.25
[mm]
4
[mm]
5
[mm]
Available Sizes: Wire 1.1
[mm], cored wire
1.6
[mm], cored wire
2.4
[mm], cored wire
2.8
[mm], cored wire
Packaging: Electrode 3.25
[mm] 4.5kg sleeves (4 sleeves=1 box)
4
[mm] 4.5kg sleeves (4 sleeves=1 box)
5
[mm] 5kg sleeves (4 sleeves=1 box)
Packaging: Wire 1.1
[mm], 15kg spools
1.6
[mm], 15kg & 25kg spools
2.4
[mm], 25kg spools
2.8
[mm], 25kg spools