Material Notes:
This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of -320°F to 350°F with and without additional lubricants.TriStar CJ Composite Bearing: Multi-layer lightweight construction provides dry lubrication with high reliability. The innermost layer features a braided synthetic fiber/PTFE tubular liner saturated with epoxy resin. A low helix angle layer of epoxy-coated glass filaments follows for axial strength. Multiple high helix angle layers comprise the outer structure and provide compressive strength. Ideally suited for non-lubricated high-load/low-speed shock load applications. Operates well in demanding and destructive environments. Rc 50 and higher steel mating surface. Material has thermal and electrical insulating properties. Suitable for use in steam, wet, dry, or vacuum environments. Markets for CJ Composite Bearings include Agricultural, Appliances, Automotive, Construction, Industrial, and Transportation.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Water Absorption <= 0.50 %

@Time 86400 sec
<= 0.50 %

@Time 24.0 hour
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
Compressive Strength 345 MPa
50000 psi
Shear Strength 34.5 MPa
5000 psi
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
Coefficient of Friction, Dynamic 0.080
0.080
Dry vs. Steel
Coefficient of Friction, Static 0.50
0.50
Dry vs. Steel
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
Unlubricated
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C
70.0 µin/in-°F
Thermal Conductivity 0.202 W/m-K
1.40 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
350 °F
Minimum Service Temperature, Air -196 °C
-320 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.41e+18 ohm-cm
2.41e+18 ohm-cm
Surface Resistance 3.93e+15 ohm
3.93e+15 ohm
Dielectric Constant 4.15

@Frequency 1.00e+6 Hz
4.15

@Frequency 1.00e+6 Hz
Dissipation Factor 0.0094

@Frequency 1.00e+6 Hz
0.0094

@Frequency 1.00e+6 Hz