Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Inhance Fluoro-Seal
Trade Name INHANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse, and creates superior adhesion between the particles and the surrounding polymerApplications: Add INHANCE UH-1000 series particles to polyurethanes, epoxies, rubber, and other polymers to create composites that capture the unique benefits of UHMWPE without the processing difficulties posed by virgin UHMWPE. These benefits include superior abrasion resistance, reduced coefficient of friction, enhanced work of fracture and improved moisture barrier. Numerous industrial parts, coatings, and other wear surfaces are now being made with these surface-activated particles. Typical incorporation levels are in the range of 10%-30% for cast parts and 5%-10% for coatingsInformation provided by Inhance/Fluoro-Seal, Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.940 g/cc
0.930 - 0.940 g/cc
Bulk Density 0.320 - 0.500 g/cc
0.0116 - 0.0181 lb/in³
Particle Size 300 µm
300 µm
Average Size
710 µm
710 µm
Finer than
Molecular Weight 3.00e+6 - 5.00e+6 g/mol
3.00e+6 - 5.00e+6 g/mol
Surface Tension 55 dynes/cm
55 dynes/cm
water wettable