MarkeTech Rutile (TiO2) Fiber Optic Crystal

Category Ceramic , Oxide , Titanium Oxide
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Rutile (TiO2) Fiber Optic Crystal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
More chemically and physically resistant than Yttrium Vanadate. Large birefringence. Used for fiber optic beam displacers and optical isolators. Grown by Vernull method. Transmission range 500 to 4500 nm.Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 4.26 g/cc
0.154 lb/in³
a Lattice Constant 4.5936 Ã…
4.5936 Ã…
c Lattice Constant 2.9852 Ã…
2.9852 Ã…
Mechanical Properties Metric English Comments
Hardness, Mohs 7.0
7.0
Thermal Properties Metric English Comments
CTE, linear 7.14 µm/m-°C
3.97 µin/in-°F
a direction
9.19 µm/m-°C
5.11 µin/in-°F
c direction
Thermal Conductivity 9.00 W/m-K
62.5 BTU-in/hr-ft²-°F
a direction
13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
c direction
Melting Point 1840 °C
3340 °F
Debye Temperature 487 °C
909 °F
Optical Properties Metric English Comments
Refractive Index 2.47
2.47
&#951; <sub>o</sub>
2.73
2.73
&#951; <sub>e</sub>
Electrical Properties Metric English Comments
Dielectric Constant 160

@Frequency 1.00e+7 Hz
160

@Frequency 1.00e+7 Hz
200

@Frequency 10000 Hz
200

@Frequency 10000 Hz
Band Gap 3.3 eV
3.3 eV
Descriptive Properties Value Comments
Crystal Structure Tetragonal
Users viewing this material also viewed the following: