Total Finaprene® 411x Styrene-Butadiene TPE Copolymer, 80 Shore A  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Styrene-Butadiene
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finaprene® 411x Styrene-Butadiene TPE Copolymer, 80 Shore A  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides excellent mechanical and elastic properties to compound.Applications: Thanks to its high molecular weight Finaprene® 411x is designed for the compounding industry. This crumb shape, along with the high molecular weight confer a quick and important oil absorption capacity to the polymer and lead tot eh production of economical compounds while keeping good mechanical properties.Additional Notes: Oil Content: 5 phr; Finaprene 1010Data provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Finaprene 2602 Test
Viscosity Measure 25 cSt
25 cSt
Toluene Solution; Finaprene 1008 Test
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Finaprene 1505 Test
Tensile Strength, Ultimate 15.0 MPa
2180 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Chemical Properties Metric English Comments
Styrene Content 31 %
31 %
Finaprene 1004 Test
Butadiene Content 69 %
69 %
Finaprene 1004 Test