Material Notes:
This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® SUPRA.Application: The steel may be used for wear exposed structures, e.g. excavating, mining and earth-moving machinery, truck dump bodies, conveying, crushing and pulverizing equipment and scrap presses.Properties typical of 15 mm plate thickness.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 1800 MPa
261000 psi
Tensile Strength, Yield 1500 MPa
218000 psi
Elongation at Break 8.0 %
8.0 %
Charpy Impact 22.0 J

@Temperature -40.0 °C
16.2 ft-lb

@Temperature -40.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.3 %
<= 1.3 %
Boron, B <= 0.0050 %
<= 0.0050 %
Carbon, C <= 0.35 %
<= 0.35 %
Chromium, Cr <= 1.3 %
<= 1.3 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni <= 1.5 %
<= 1.5 %
Other <= 0.78 %
<= 0.78 %
Carbon Equivalent
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.80 %
<= 0.80 %
Sulfur, S <= 0.012 %
<= 0.012 %