Teknor Apex Sinvicomp SGH 4500 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SGH 4500 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength, Yield 18.6 MPa
2700 psi
9.8 in/min; ASTM D638
Elongation at Break 300 %
300 %
9.8 in/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time >=1800 sec
374 °F

@Time >=0.500 hour
Congo Red; BS 2782