| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade | 
| Manufacturer | Teknor Apex Company | 
| Trade Name | APEX® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Teknor Apex APEX® 80128-Y Polyvinyl Chloride, Flexible.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 86 | 86 | 15 seconds; ASTM D2240 | 
| Tensile Strength at Break | 17.9 MPa | 2590 psi | ASTM D638 | 
| Elongation at Break | 310 % | 310 % | ASTM D638 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous Use; ASTM D794 | 
| Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 | 
| Oxygen Index | 24 % | 24 % | ASTM D2863 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 3.20e+13 ohm-cm | 3.20e+13 ohm-cm | ASTM D257 | 
| Dielectric Constant |           3.35                     @Frequency 1.00e+6 Hz  | 
                  3.35                     @Frequency 1.00e+6 Hz  | 
        ASTM D150 | 
|           5.01                     @Frequency 1000 Hz  | 
                  5.01                     @Frequency 1000 Hz  | 
        ASTM D150 | |
| Dissipation Factor |           0.069                     @Frequency 1.00e+6 Hz  | 
                  0.069                     @Frequency 1.00e+6 Hz  | 
        ASTM D150 | 
|           0.085                     @Frequency 1000 Hz  | 
                  0.085                     @Frequency 1000 Hz  | 
        ASTM D150 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Appearance | Opaque |