Material Notes:
Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications; Toys; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
15 seconds; ASTM D2240
Tensile Strength at Break 16.2 MPa
2350 psi
ASTM D638
Tensile Strength 6.89 MPa

@Strain 100 %
1000 psi

@Strain 100 %
ASTM D638
Elongation at Break 470 %
470 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -38.0 °C
-36.4 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Descriptive Properties Value Comments
Appearance Clear