Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mearthane Durethaneâ„¢ S DS-330A Solid Polyurethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mearthane Products Corporation (MPC)
Trade Name Durethane™ S
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Mearthane Durethaneâ„¢ S DS-330A Solid Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, elongation, coefficient of friction, abrasion resistance, compression set, compression modulus, tensile modulus, resilience, solvent resistance and color.Applications: Mearthane will custom-manufacture industrial product, wheels, and other components to customer specifications. Durethane S is a machinable to fine surface finishes. Typical applications include: rollers pads, bumpers, and other components in paper handling mechanisms for business machines such as: printers, copiers, fax machines, postage meters, collators, and ATMs. Other applications include: inline skatewheels, skateboard wheels, castors, shock absorbers, springs and elastomeric die blocks.Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.Information provided by Mearthane Products Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
ASTM D2240
Elongation at Break 1100 %
1100 %
ASTM D412
100% Modulus 0.000552 GPa
0.0801 ksi
ASTM D412
Tear Strength 14.9 kN/m
85.0 pli
Die C; ASTM D624
Compression Set 5.0 %

@Temperature 70.0 °C
5.0 %

@Temperature 158 °F
22 hours; ASTM D395B