Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Compressive Strength 138 MPa
20000 psi
ASTM D695
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
ASTM D648