Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0035 cm/cm

@Thickness 3.17 mm
0.0035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 4.07 GPa
590 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
30.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
265 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed; ASTM D648
Flammability, UL94 HB