| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Conductive |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® M-2386 NAT Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
| Water Absorption | 0.12 % | 0.12 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 107 MPa | 15500 psi | ASTM D638 |
| Elongation at Break | 2.8 % | 2.8 % | ASTM D638 |
| Flexural Strength | 145 MPa | 21000 psi | ASTM D790 |
| Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
| Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 290 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | 1000 ohm | 1000 ohm | ASTM D648 |