| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® J-1200/CF/15/V0/ND BK2089 ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Water Absorption | 0.30 % | 0.30 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.00050 cm/cm | 0.00050 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 100 MPa | 14500 psi | ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
| Tensile Modulus | 11.0 GPa | 1600 ksi | ASTM D638 |
| Flexural Strength | 148 MPa | 21500 psi | ASTM D790 |
| Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
| Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 18.0 µm/m-°C @Temperature 20.0 °C |
10.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 96.1 °C | 205 °F | ASTM D648 |