Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N220 (ISAF) Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N220 (ISAF) Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5N220 (ISAF)20All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Yield 27.89 MPa
4045 psi
Elongation at Yield 493 %
493 %
100% Modulus 0.00299 GPa
0.433 ksi
200% Modulus 0.00673 GPa
0.976 ksi
300% Modulus 0.01180 GPa
1.711 ksi
Tear Strength 45.5 kN/m
260 pli
Die C
Taber Abrasion, mg/1000 Cycles 0.050
0.050
H-18, mg loss/rev
Compression Set 61 %

@Temperature 70.0 °C,
Time 79200 sec
61 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 149 °C
0.333 hour

@Temperature 300 °F
Users viewing this material also viewed the following: