Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged

Category Metal , Nonferrous Metal , Titanium Alloy , Alpha/Beta Titanium Alloy
Manufacturer TIMET
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET.
Physical Properties Metric English Comments
Density 4.53 g/cc
0.164 lb/in³
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1205 MPa
174800 psi
Typical
Tensile Strength, Yield 1105 MPa

@Strain 0.200 %
160300 psi

@Strain 0.200 %
Typical
Elongation at Break 8.0 %
8.0 %
Typical
Modulus of Elasticity 115 GPa
16700 ksi
(Annealed)
Thermal Properties Metric English Comments
Beta Transus 945 °C
1730 °F
Component Elements Properties Metric English Comments
Aluminum, Al 6.0 %
6.0 %
Copper, Cu 0.50 %
0.50 %
Iron, Fe 0.50 %
0.50 %
Tin, Sn 2.0 %
2.0 %
Titanium, Ti 85 %
85 %
Calculated as remainder
Vanadium, V 6.0 %
6.0 %
Users viewing this material also viewed the following: