TIMCAL TIMREX® M80 mesh FR Natural Flake Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® M80 mesh FR Natural Flake Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-des-Îles, Quebec, Canada. Further processing can be done either in Lac-des-Îles or for high added value products (e.g. TIMREX PG25) in our new processing plant in Terrebonne, Quebec, Canada. All TIMREX“Naturals” are thoroughly controlled in our laboratories to ensure quality, consistency and total customer satisfaction.Advantages and applications: Suitable for all organic bonded friction materials, especially for linings in drum brakes as well as in brake pads for trains. Good transfer film formationGood thermal conductivityExcellent lubricating propertiesInformation provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.690 g/cc
0.0249 lb/in³
Tap
Particle Size 80 µm
80 µm
Deformation 1.2 %
1.2 %
elastic
5.2 %
5.2 %
plastic
6.4 %
6.4 %
plastic + elastic
Ash 4.0 - 6.0 %
4.0 - 6.0 %
Guaranteed
<= 7.0 %
<= 7.0 %
Thermal Properties Metric English Comments
Thermal Conductivity 190 W/m-K
1320 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
Guaranteed
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Crystallite height Lc >350 nm
DBP absorption 37 g/100g
(Dibutylphthalate)