Buckeye Polymers BP RPP 2010 T NAT Polypropylene, Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 2010 T NAT Polypropylene, Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents. Buckeye Polymers can also customize these materials through the addition of UV packages, custom color matching, and processing additives.Product Features:Increased stiffness and heat deflectionGood UV resistanceIndustrial, appliance, construction marketsGood scratch and mar resistanceAppearance: NaturalForms: PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
Melt Flow 10 - 14 g/10 min
10 - 14 g/10 min
ASTM D1238
Ash 18 - 22 %
18 - 22 %
ASTM D5630
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.72 GPa
>= 250 ksi
ASTM D790
Izod Impact, Notched >= 0.427 J/cm
>= 0.800 ft-lb/in
ASTM D256