Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech RJ72470 PVC and Alloy Products for Wire and Cable

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech RJ72470 PVC and Alloy Products for Wire and Cable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Spartech
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.6 °C
105 °F
Descriptive Properties Value Comments
Wire Style specialty compounds