Material Notes:
Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It has high flexibility and very high impact strength. It is specially available for pipes extrusion.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ISO 527 type 1 A
Elongation at Break 270 %
270 %
ISO 527 Type 1A
Tensile Modulus 0.400 GPa
58.0 ksi
ISO 527 Type 1A
Flexural Strength 20.0 MPa
2900 psi
ISO 178
Flexural Modulus 0.380 GPa
55.1 ksi
ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243
Dissipation Factor 0.12
0.12
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %