Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other solid particles. The grades differ by their molecular weights, with 3000P the highest and 3600P the lowest. There is a direct correlation between molecular weight and solution viscosity. PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water, and mineral acids. Cast films or coatings of PESU are transparent and have additional desirable properties including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance. Typical applications include high-temperature coating formulations, membranes, advanced high-temperature composites, and specialty adhesives.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Viscosity 275 cP

@Temperature 40.0 °C
275 cP

@Temperature 104 °F
25% in dimethylacetamide; Internal Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.0 µm/m-°C
27.2 µin/in-°F
ASTM D696
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Agency Ratings NSF 51
Maximum Temperature of Use: 124°C (356°F)
Appearance Transparent - Slight Yellow
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Acid Resistant
Flame Retardant
Food Contact Acceptable
Good Adhesion
Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Thermal Stability
Good Toughness
High Flow
High Heat Resistance
High Tensile Strength
Hydrolysis Resistant
Low Molecular Weight
Medium Rigidity
Forms Granules
Powder
Generic PESU
Processing Method Coating
Solution Processing
Spraying
Residual Solvent (%) 0.5
Internal Method
RoHS Compliance RoHS Compliant
Uses Adhesives
Binder
Coating Applications
Compounding
Users viewing this material also viewed the following: