Solvay Specialty Polymers Polymist® XPP 527 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Polymist®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® XPP 527 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® XPP 527 a white PTFE micronized powder PTFE micronized powder composed of discrete particles. Designed for use in high end performance Coatings applications, Polymist® XPP 527 will improve non-stick properties and mar and abrasion resistance.Main features of Polymist® XPP 527 are Improved abrasion, scratch and rub resistance, Increased slip and surface lubricity, Reduced blocking, Better chemical resistance, Increased temperature resistance, Gloss retentionUses: AdditiveAdditional Properties: Bulk Density - ASTM D4895 500 g/l; Melt Temperature - ASTM D3418 315 to 325 °C; Particle Size - Internal Method 30.0 µm; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder