Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Kadel® E-1300 Polyketone  (discontinued **)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Kadel® E-1300 Polyketone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical resistance for application in hostile environments.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 214 MPa
31000 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Flexural Yield Strength 288 MPa
41800 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Tensile Impact Strength 180 kJ/m²
85.7 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
<br>@Temperature 20.0 °C
5.56 µin/in-°F
<br>@Temperature 68.0 °F
ASTM E381
Deflection Temperature at 1.8 MPa (264 psi) 324 °C
615 °F
ASTM D648
Flammability, UL94 V-0
<br>@Thickness 0.800 mm
V-0
<br>@Thickness 0.0315 in
V-0
<br>@Thickness 0.800 mm
V-0
<br>@Thickness 0.0315 in
Copyright © lookpolymers.com All Rights Reserved