| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | Kazanorgsintez |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Kazanorgsintez PC-003 Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | <= 0.792 g/cc | <= 0.0286 lb/in³ | 2nd Grade |
| Melt Flow | 1.5 - 3.5 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
1.5 - 3.5 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | >= 55.0 MPa | >= 7980 psi | 2nd Grade |
| >= 58.0 MPa | >= 8410 psi | 1st Grade | |
| >= 60.0 MPa | >= 8700 psi | Superior Quality | |
| Elongation at Break | >= 75 % | >= 75 % | 2nd Grade |
| >= 90 % | >= 90 % | Superior Quality, 1st Grade | |
| Flexural Modulus | 2.00 GPa | 290 ksi | 2nd Grade |
| 2.25 GPa | 326 ksi | Superior Grade, 1st Grade | |
| Transverse Strength | >= 80.0 MPa | >= 11600 psi | 2nd Grade, at max sample load |
| >= 90.0 MPa | >= 13100 psi | Superior Quality, 1st Grade, at max sample load | |
| Compressive Yield Strength | >= 68.0 MPa | >= 9860 psi | 1st Grade, 2nd Grade |
| >= 74.0 MPa | >= 10700 psi | Superior Quality | |
| Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 2nd Grade |
| 66.0 kJ/m² | 31.4 ft-lb/in² | Superior Grade, 1st Grade |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | >= 147 °C | >= 297 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Yellow Index | 1.0 - 2.5 % | 1.0 - 2.5 % | Superior Grade |
| Transmission, Visible | 82 % | 82 % | 2nd Grade |
| 86 % | 86 % | Superior Quality, 1st Grade | |
| >= 89 % | >= 89 % | Superior Grade, 1st Grade |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Free Water | <= 0.50 % | <= 0.50 % | 1st Grade |
| <= 0.80 % | <= 0.80 % | 2nd Grade |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Mass Content (%) | 0.002 | Mass content of acids as defined by acetic acid, 1st Grade |
| 0.003 | Mass content of acids as defined by acetic acid, 2nd Grade | |
| 99 | Mass content of acetone, 2nd Grade | |
| 99.5 | Mass content of acetone, 1st Grade | |
| 99.75 | Mass content of acetone, Premium Grade | |
| Turbidity | 1 | Superior Grade, 1st Grade |