Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Solvay Specialty Polymers
Trade Name Algoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber since it allows good degassing during the sintering process.Features: Good Chemical ResistanceUses: Additive; BlendingInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 2.17 g/cc
0.0784 lb/in³
ASTM D792
Apparent Bulk Density 0.380 g/cc
0.0137 lb/in³
ASTM D4894
Water Absorption 0.00 %
0.00 %
ASTM D570
Particle Size 15 µm
15 µm
Internal Method
Linear Mold Shrinkage 0.030 cm/cm
0.030 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service
Flammability, UL94 V-0
V-0
VE-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Dielectric Constant 2.1

@Frequency 60.0 - 2.00e+9 Hz
2.1

@Frequency 60.0 - 2.00e+9 Hz
ASTM D150
Dielectric Strength 70.0 kV/mm
1780 kV/in
Estimated from similar grades. ASTM D149
Dissipation Factor >= 0.00030

@Frequency 60.0 - 2.00e+9 Hz
>= 0.00030

@Frequency 60.0 - 2.00e+9 Hz
ASTM D150
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1550
Availability Asia Pacific; Europe
Color White
Form Powder
Users viewing this material also viewed the following: