Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay RHODAPHOSE® PHENYL DICHLOROPHOSPHATE Phosphorus Derivative

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPHOSE® PHENYL DICHLOROPHOSPHATE Phosphorus Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Intermediate in selective manufacturing of phosphoric acid diesters; protective agent for hydroxyl groups.Identification: PHENYL DICHLOROPHOSPHATECAS: 770 – 12 – 7Available in: Asia Pacific, Europe, Latin America and North America Identity: Conforms, AM6100Applications: PHENYL DICHLOROPHOSPHATE is used as phosphorylating agent for alcohols/amines in conjunction with a coupling agent in the production of pharmaceutical intermediatesInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Descriptive Properties Value Comments
Appearance Clear colorless liquid
Composition Phenol
>0.5%, AM6100
Phenyl dichlorophosphate
>98%, AM6412
Foreign Matter Free from particulate matter