Material Notes:
Identification: POLYOXYETHYLENE PHENYL ESTER PHOSPHATE ACID FORMCAS: 39464 – 70 – 5Solublility: Readily soluble in water, ketones, alcohols and glycol ether solvents. Soluble in strong caustic solutions. Insoluble in hydrocarbon and halogenated solvents.Available in: Asia Pacific, Europe and Latin America Applications: Hydrotropic agent. Metal working: extreme-pressure additive for the formulation of soluble oils, synthetic and semi-synthetic fluids, cleaning fluids. This product is non-foaming.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
pH 2.2
2.2
5% aq. Sol.
Chemical Properties Metric English Comments
Total Acid Number 245 - 270
245 - 270
[mg KOH/g]; RPG44
Processing Properties Metric English Comments
Moisture Content 28 - 32 %
28 - 32 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Pale yellow liquid
Cloud Point >100°C
1% in 25% NAOH
Ionic Charge Anionic
Setting point <0°C