Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Potassium Hydrogen Fluoride

Category Ceramic , Halide
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Potassium Hydrogen Fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Potassium hydrogenfluoride (KHF2) is used in the chemical industry, manufacture of wood preservatives glass processing, glass manufacturing, and for the production of soldering agents. Potassium hydrogendifluoride: CAS-No.: 7789-29-9 / EC-No.: 232-156-2 / Index-No.: 009-008-00-9Uses: Chemical industry, Metal treatment, Welding and soldering agents and Chemical intermediateInformation provided by Solvay
Physical Properties Metric English Comments
Molecular Weight 78 g/mol
78 g/mol
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
Descriptive Properties Value Comments
Appearance powder, crystalline, hygroscopic
Color white
Composition 0.99
Potassium hydrogendifluoride
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved