Shakespeare WP-200 diameter 0.2 mm Weft Polyester Monofilament

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WP-200 diameter 0.2 mm Weft Polyester Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Paper Machine Clothing MonofilamentStandard molecular weightPolyesterModerate ModulusModerate shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break 738 MPa
107000 psi
Elongation at Break 23 %
23 %
Elongation at Yield 5.5 %
5.5 %
at 3 g/D
Thermal Properties Metric English Comments
Shrinkage 10.0 %

@Temperature 175 °C
10.0 %

@Temperature 347 °F