Solvay Chemicals Oxyper® S142 Sodium Percarbonate

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name Oxyper®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Oxyper® S142 Sodium Percarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automatic machine dishwash powders and tablets. Oxyper® S142 combines the properties of hydrogen peroxide with the properties of sodium carbonate in an easy to use free flowing white granular powder with excellent water solubility and high rate of dissolution. The bleaching action of Oxyper® S142 maintains fabric whiteness and color brightness while effectively removing wine, fruit, coffee, tea and other stains without damaging fibers. The alkalinity, the buffering capacity and water softening properties of sodium carbonate provide additional cleaning benefits, such as helping the removal of natural fatty soils. EINECS Number: 239-707-6/CAS Number: 15630-89-4Information provided by Solvay
Physical Properties Metric English Comments
Bulk Density 0.900 - 1.20 g/cc
0.0325 - 0.0434 lb/in³
Solubility in Water 15 %
15 %
at 20°C
17.5 %
17.5 %
at 30°C
Particle Size <= 150 µm
<= 150 µm
<2%
650 - 900 µm
650 - 900 µm
Mean particle size
>= 1400 µm
>= 1400 µm
<10%
>= 1600 µm
>= 1600 µm
<3%
pH 10.4 - 10.6
10.4 - 10.6
1% solution
Molecular Weight 314 g/mol
314 g/mol
Descriptive Properties Value Comments
Appearance White, crystalline granules
Composition >13%
Available Oxygen (AvOx)
Rate of dissolution >90%
after 2 min, 2g/l; 15°C water