Material Notes:
CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2 Applications: Chemical industry, oil industry, civil engineering, dust control, winter road, environment, industrial and domestic drying and tartaric acidInformation provided by Solvay
Physical Properties Metric English Comments
Density <= 0.800 g/cc

@Temperature 0.900 °C
<= 0.0289 lb/in³

@Temperature 33.6 °F
Molecular Weight 147.02 g/mol
147.02 g/mol
Descriptive Properties Value Comments
Appearance White or Off-white flakes
Composition 0.7 g/kg
Water insoluble
0.9 g/kg
Ca(OH)2
1.02
CaCl2.2H2O
1.9 g/kg
SO4
26 g/kg
NaCl
6 mg/kg
Fe
750-810 g/kg
CaCl2, Specifications
771 g/kg
CaCl2
99-107%
CaCl2.2H2O, Specifications
Granulometry 0.003
<0.5 mm, statistical average
0.006
<1.0 mm, statistical average
0.02
<0.5 mm, typical value
0.03
<1.0 mm, typical value
0.03
<2.0 mm, statistical average
0.11
<2.0 mm, typical value
0.5
<4.0 mm, statistical average
0.96
<4.0 mm, typical value
0.99
<8.0 mm, statistical average
1
<8.0 mm, typical value
1
<10.0 mm, statistical average
1
<10.0 mm, typical value