Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene

Category Fluid
Manufacturer Solvay Chemicals
Trade Name Allyl chloride
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6/CAS Number: 107-05-1/UN number: 1100Information provided by Solvay
Physical Properties Metric English Comments
Density 0.7911 g/cc

@Pressure 0.7726 MPa,
Temperature 120 °C
0.02858 lb/in³

@Pressure 112.1 psi,
Temperature 248 °F
0.8084 g/cc

@Pressure 0.6201 MPa,
Temperature 110 °C
0.02921 lb/in³

@Pressure 89.94 psi,
Temperature 230 °F
0.825 g/cc

@Pressure 0.4912 MPa,
Temperature 100 °C
0.0298 lb/in³

@Pressure 71.24 psi,
Temperature 212 °F
0.8411 g/cc

@Pressure 0.3835 MPa,
Temperature 90.0 °C
0.03039 lb/in³

@Pressure 55.62 psi,
Temperature 194 °F
0.8565 g/cc

@Pressure 0.2947 MPa,
Temperature 80.0 °C
0.03094 lb/in³

@Pressure 42.74 psi,
Temperature 176 °F
0.8714 g/cc

@Pressure 0.2226 MPa,
Temperature 70.0 °C
0.03148 lb/in³

@Pressure 32.29 psi,
Temperature 158 °F
0.8859 g/cc

@Pressure 0.1649 MPa,
Temperature 60.0 °C
0.03201 lb/in³

@Pressure 23.92 psi,
Temperature 140 °F
0.8999 g/cc

@Pressure 0.1196 MPa,
Temperature 50.0 °C
0.03251 lb/in³

@Pressure 17.35 psi,
Temperature 122 °F
0.9136 g/cc

@Pressure 0.0848 MPa,
Temperature 40.0 °C
0.03301 lb/in³

@Pressure 12.3 psi,
Temperature 104 °F
0.9203 g/cc

@Pressure 0.0707 MPa,
Temperature 35.0 °C
0.03325 lb/in³

@Pressure 10.3 psi,
Temperature 95.0 °F
0.9269 g/cc

@Pressure 0.0585 MPa,
Temperature 30.0 °C
0.03349 lb/in³

@Pressure 8.48 psi,
Temperature 86.0 °F
0.9334 g/cc

@Pressure 0.0481 MPa,
Temperature 25.0 °C
0.03372 lb/in³

@Pressure 6.98 psi,
Temperature 77.0 °F
0.9398 g/cc

@Pressure 0.0392 MPa,
Temperature 20.0 °C
0.03395 lb/in³

@Pressure 5.69 psi,
Temperature 68.0 °F
0.9462 g/cc

@Pressure 0.0317 MPa,
Temperature 15.0 °C
0.03418 lb/in³

@Pressure 4.60 psi,
Temperature 59.0 °F
0.9525 g/cc

@Pressure 0.0254 MPa,
Temperature 10.0 °C
0.03441 lb/in³

@Pressure 3.68 psi,
Temperature 50.0 °F
0.9587 g/cc

@Pressure 0.0202 MPa,
Temperature 5.00 °C
0.03464 lb/in³

@Pressure 2.93 psi,
Temperature 41.0 °F
0.9648 g/cc

@Pressure 0.0159 MPa,
Temperature 0.000 °C
0.03486 lb/in³

@Pressure 2.31 psi,
Temperature 32.0 °F
0.9709 g/cc

@Pressure 0.0124 MPa,
Temperature -5.00 °C
0.03508 lb/in³

@Pressure 1.80 psi,
Temperature 23.0 °F
0.9769 g/cc

@Pressure 0.00950 MPa,
Temperature -10.0 °C
0.03529 lb/in³

@Pressure 1.38 psi,
Temperature 14.0 °F
0.9828 g/cc

@Pressure 0.00720 MPa,
Temperature -15.0 °C
0.03551 lb/in³

@Pressure 1.04 psi,
Temperature 5.00 °F
0.9887 g/cc

@Pressure 0.00540 MPa,
Temperature -20.0 °C
0.03572 lb/in³

@Pressure 0.783 psi,
Temperature -4.00 °F
1.0003 g/cc

@Pressure 0.00290 MPa,
Temperature -30.0 °C
0.036138 lb/in³

@Pressure 0.421 psi,
Temperature -22.0 °F
Solubility in Water 0.36 %
0.36 %
Viscosity 0.34 cP
0.34 cP
Molecular Weight 76.53 g/mol
76.53 g/mol
Vapor Pressure 0.400 bar
300 torr
Surface Tension 0.023 dynes/cm
0.023 dynes/cm
Thermal Properties Metric English Comments
Specific Heat Capacity 0.950 J/g-°C
0.227 BTU/lb-°F
vapor
1.50 J/g-°C
0.359 BTU/lb-°F
liquid
Melting Point -135 °C
-211 °F
Freezing Point
Boiling Point 43.0 °C
109 °F
Azeotrope with water
45.0 °C

@Pressure 1.013 MPa
113 °F

@Pressure 146.9 psi
Decomposition Temperature >= 80.0 °C
>= 176 °F
Flash Point -27.0 °C
-16.6 °F
TAG closed cup
Electrical Properties Metric English Comments
Dielectric Constant 1.013

@Temperature 19.0 °C
1.013

@Temperature 66.2 °F
vapor
8.2

@Temperature 20.0 °C
8.2

@Temperature 68.0 °F
liquid
Chemical Properties Metric English Comments
Critical Pressure 48.0 bar
36000 torr
Critical Temperature 241 °C
466 °F
Descriptive Properties Value Comments
Appearance Clear liquid, free from visible matter or particles
Auto-ignition temperature >392°C
Coefficient of volume expansion 0.0014
K<sup>-1</sup>
Combustion heat 24 kJ/g
Composition <100 mg/kg
Water, ASTM D3401, ASTM E1064
>99%
Allyl Chloride - assay
22 g/kg
Azetrope with water, content
Flammability limits 3.3-11.2%
Latent heat of evaporation 0.37 kJ/g
45°C
Partition coefficient P 2.1 Log P o/w
n-octanol.water
Solubility of water in organic 0.8 g/kg
Users viewing this material also viewed the following: