| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler |
| Manufacturer | Sichuan Deyang Chemical Co. Ltd. |
| Trade Name | Haton® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Sichuan Deyang Haton® hCF31 Polyphenylene Sulfide.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | GB/T 1033.1-2008 |
| Water Absorption | 0.020 % | 0.020 % | GB/T 1034-2008 |
| Linear Mold Shrinkage, Flow | 0.0012 cm/cm | 0.0012 in/in | GB/T 15585-1995 |
| Linear Mold Shrinkage, Transverse | 0.0026 cm/cm | 0.0026 in/in | GB/T 15585-1995 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 108 | 108 | GB/T 3398.2-2008 |
| Tensile Strength | 176 MPa | 25500 psi | GB/T 1040.2-2006 |
| Elongation at Break | 0.80 % | 0.80 % | GB/T1040.2-2006 |
| Flexural Strength | 256 MPa | 37100 psi | GB/T 9341-2008 |
| Flexural Modulus | 21.2 GPa | 3070 ksi | GB/T 9341-2008 |
| Izod Impact, Notched (ISO) | 8.60 kJ/m² | 4.09 ft-lb/in² | GB/T 1843-2008 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
| Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 511 °F | GB/T 1634.2-2004 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Insulation Resistance | 1.00e+9 ohm | 1.00e+9 ohm | GB/T 10064-2006 |