Sibur SKN-33PVC-30 Nitrile-Butadiene Rubber (NBR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur SKN-33PVC-30 Nitrile-Butadiene Rubber (NBR).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
For production of rubber and asbestos technical articles which are used as sets for automobile, air planes, different machines and equipment, agricultural, drilling, and polygraph machinery, as well as for production of glues, mastics, and sheaths for cables and shoes.
Physical Properties Metric English Comments
Mooney Viscosity 60 - 80

@Temperature 100 °C
60 - 80

@Temperature 212 °F
ML 1-4
Ash <= 1.0 %
<= 1.0 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 19.6 MPa
>= 2840 psi
Elongation at Break >= 400 %
>= 400 %
Descriptive Properties Value Comments
Loss During Drying <1%
Mass Share of Combined Nitrile and Acrylic Acid 28-32%
Mass Share of Ionol >0.5%