Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ShinEtsu X65130 U is a black semiconductive silicone compound designed to give very low volume resistivity for molding and extruding. Product Features: Good processability.Lower than average volume resistivity.Typical Applications: EMI gaskets.Key pads.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
DCBP Cure
1.28 g/cc
1.28 g/cc
DBPH Cure
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
DCBP Cure
71
71
DBPH Cure
Tensile Strength at Break 4.59 MPa
665 psi
DBPH Cure
4.79 MPa
695 psi
DCBP Cure
Elongation at Break 130 %
130 %
DCBP Cure
130 %
130 %
DBPH Cure
Tear Strength 12.3 kN/m
70.0 pli
Die B; DCBP Cure
13.1 kN/m
75.0 pli
Die B; DBPH Cure
Compression Set 20 %

@Temperature 180 °C,
Time 79200 sec
20 %

@Temperature 356 °F,
Time 22.0 hour
DCBP Cure
Descriptive Properties Value Comments
Cure Agent DBPH
DBPH-50
Cure Type Press Cure
Users viewing this material also viewed the following: