Shin-Etsu Silicones X-52-2259 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Shin-Etsu Silicones X-52-2259 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Solids Content 60 %
60 %
Viscosity Measure 4000 cSt
4000 cSt
Emulsion
75000 cSt
75000 cSt
Descriptive Properties Value Comments
Appearance Emulsion
Diluent (%) NA
Surfactant Non-ionic