Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, filling compounds, etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 001-2003Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Specific Gravity 2.13 - 2.16 g/cc
2.13 - 2.16 g/cc
Bulk Density 0.300 - 0.450 g/cc
0.0108 - 0.0163 lb/in³
Particle Size 65 µm
65 µm
<3%
Mechanical Properties Metric English Comments
Tensile Strength >= 27.4 MPa
>= 3970 psi
Qualified
>= 29.0 MPa
>= 4210 psi
Grade A
Elongation at Break >= 280 %
>= 280 %
Qualified
>= 300 %
>= 300 %
Grade A
Thermal Properties Metric English Comments
Melting Point 322 - 332 °C
612 - 630 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 60.0 kV/mm
>= 1520 kV/in
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
For Check Execute according to requirement of HQ/T2903-1997
For Process For Molding
Smoothness & Cleanliness White sheet surface, even texture, no metal residue quantity (<0.5mm)<2
Thermal Inst. Index <20