Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shakespeare Sanstat® CN125 .64mm Nylon 66 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66 Fiber
Manufacturer Shakespeare Company
Trade Name Sanstat®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Sanstat® CN125 .64mm Nylon 66 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.11 g/cc

@Diameter 0.640 mm
0.0401 lb/in³

@Diameter 0.0252 in
Product yield of 2792 m/kg.
Fiber Count 3580 dtex
3220 denier
Per Filament
Mechanical Properties Metric English Comments
Elongation at Break 26 %
26 %
Tenacity 0.441 N/tex
5.00 g/denier
14.5 kg breaking load
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
Shrinkage 5.00 %

@Temperature 175 °C,
Time 601 sec
5.00 %

@Temperature 347 °F,
Time 0.167 hour
Electrical Properties Metric English Comments
Electrical Resistivity 5000 ohm-cm
5000 ohm-cm
Average
<= 8000 ohm-cm
<= 8000 ohm-cm