| Category | Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) | 
| Manufacturer | Seals Eastern, Inc | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Seals Eastern 5722 Fluorocarbon-Elastomer.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D297, 15 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | >= 50 | >= 50 | ASTM D2240, Type A | 
| 60 | 60 | AVG; ASTM D2240, Type A | |
| Tensile Strength at Break | >= 8.96 MPa | >= 1300 psi | ASTM D412 Method A | 
| 12.59 MPa | 1826 psi | AVG; ASTM D412 Method A | |
| Tensile Strength, Yield | >= 0.986 MPa | >= 143 psi | Stress at Elongation M50; ASTM D412 Method A | 
| 1.14 MPa | 165 psi | AVG Stress at Elongation M50; ASTM D412 Method A | |
| >= 1.45 MPa | >= 211 psi | Stress at Elongation M100; ASTM D412 Method A | |
| 1.59 MPa | 231 psi | AVG Stress at Elongation M100; ASTM D412 Method A | |
| Elongation at Break | >= 174 % | >= 174 % | ASTM D412 Method A | 
| 433 % | 433 % | AVG; ASTM D412 Method A | |
| Tear Strength Test | 141 | 141 | (psi); ASTM D624, Die B | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Strain Energy / Unit Volume at 20% Elongation (psi) | 13 |