Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott WG295 Long Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott WG295 Long Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG665, RG695, RG715, RG780, RG830, RG850, RG1000, WG225, WG280, GG385, WG305, WG320
Physical Properties Metric English Comments
Density 2.51 g/cc
0.0907 lb/in³
Thermal Properties Metric English Comments
CTE, linear 3.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.11 µin/in-°F

@Temperature -22.0 - 158 °F
4.10 µm/m-°C

@Temperature 20.0 - 300 °C
2.28 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 557 °C
1030 °F
Glass Temperature Coefficient 0.020
0.020
Optical Properties Metric English Comments
Refractive Index 1.51

@Wavelength 1014 nm
1.51

@Wavelength 1014 nm
Hg
1.52

@Wavelength 587.6 nm
1.52

@Wavelength 587.6 nm
He
1.54

@Wavelength 334.1 nm
1.54

@Wavelength 334.1 nm
Hg
Transmission, Visible 92 %

@Wavelength 400 - 700 nm
92 %

@Wavelength 400 - 700 nm
Internal transmittance of 100%  from 400-700 nm.
IR Transmittance 92 %

@Wavelength 700 - 1600 nm
92 %

@Wavelength 700 - 1600 nm
Internal transmittance of 100%  from 700-1600 nm.
UV Transmittance <= 0.060 %

@Wavelength 200 - 270 nm
<= 0.060 %

@Wavelength 200 - 270 nm
92 %

@Wavelength 360 - 390 nm
92 %

@Wavelength 360 - 390 nm
Internal transmittance of 100%  from 360-390 nm
Reflection Coefficient, Visible (0-1) 0.93
0.93
Chemical Properties Metric English Comments
Acid Class, SR 51.3
51.3
Alkali Class, AR 3.3
3.3
Stain Resistance Class, FR 3
3
Users viewing this material also viewed the following: