Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott UG11 Band Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott UG11 Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.92 g/cc
0.105 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.33 µin/in-°F

@Temperature -22.0 - 158 °F
9.00 µm/m-°C

@Temperature 20.0 - 300 °C
5.00 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 545 °C
1010 °F
Optical Properties Metric English Comments
Refractive Index 1.56

@Wavelength 587.6 nm
1.56

@Wavelength 587.6 nm
He
1.59

@Wavelength 365 nm
1.59

@Wavelength 365 nm
Hg
Transmission, Visible <= 1.0 %

@Wavelength 400 - 680 nm
<= 1.0 %

@Wavelength 400 - 680 nm
20 %

@Wavelength 700 nm
20 %

@Wavelength 700 nm
Internal transmittance of 22% at 700 nm
IR Transmittance 26 %

@Wavelength 720 nm
26 %

@Wavelength 720 nm
Internal transmittance of 28% at 720 nm.
UV Transmittance <= 0.060 %

@Wavelength 200 - 240 nm
<= 0.060 %

@Wavelength 200 - 240 nm
84 %

@Wavelength 320 - 340 nm
84 %

@Wavelength 320 - 340 nm
Internal transmittance of 93% at 330 nm
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 3
3
Alkali Class, AR 2.2
2.2
Stain Resistance Class, FR 0.0
0.0