Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® XP-2165MC PPS

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® XP-2165MC PPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.96 g/cc
1.96 g/cc
ASTM D792
Water Absorption 0.020 %

@Temperature 23.0 °C
0.020 %

@Temperature 73.4 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0080 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 147 MPa
21300 psi
5 mm/min; ASTM D638
Elongation at Break 1.5 %
1.5 %
5 mm/min; ASTM D638
Flexural Strength 196 MPa
28400 psi
2.8 mm/min; ASTM D638
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 270 °C

@Thickness 6.40 mm
518 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
5VB

@Thickness 1.60 mm
5VB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
50% RH; ASTM D257
Dielectric Constant 5.0

@Frequency 1.00e+6 Hz
5.0

@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.0070

@Frequency 1.00e+6 Hz
0.0070

@Frequency 1.00e+6 Hz
ASTM D150