Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

STAR Thermoplastic Alloys & Rubbers StarGrip GP 30-9000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarGrip
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF STAR Thermoplastic Alloys & Rubbers StarGrip GP 30-9000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: StarGrip GP 30-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery FeelHigh TackinessNon-slipProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Viscosity 5000 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
5000 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 31

@Time 10.0 sec
31

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 3.10 MPa

@Time 7200 sec
450 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 995 %

@Time 7200 sec
995 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.000931 GPa

@Time 7200 sec
0.135 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 11.0 kN/m
63.0 pli
ASTM D624
Descriptive Properties Value Comments