STAR Thermoplastic Alloys & Rubbers StarFlex® P 7190-1000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarFlex®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF STAR Thermoplastic Alloys & Rubbers StarFlex® P 7190-1000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: StarFlex P 7190-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades availableProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ASTM D792
Viscosity 10900 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
10900 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 92

@Time 10.0 sec
92

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 12.82 MPa

@Time 7200 sec
1859 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 705 %

@Time 7200 sec
705 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00503 GPa

@Time 7200 sec
0.730 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 46.8 kN/m
267 pli
ASTM D624
Descriptive Properties Value Comments
Color Natural