Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SSAB Tunnplat Docol® 1000 DL High-strength Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Docol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Docol® 1000 DL High-strength Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
In course of development.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1000 - 1200 MPa
145000 - 174000 psi
Tensile Strength, Yield >= 650 MPa
>= 94300 psi
After bake hardening
500 - 750 MPa

@Strain 0.200 %
72500 - 109000 psi

@Strain 0.200 %
Elongation at Break >= 8.0 %
>= 8.0 %
A<sub>80</sub>
Bend Radius, Minimum >= 3.0 t
>= 3.0 t
90° bend
Component Elements Properties Metric English Comments
Aluminum, Al 0.040 %
0.040 %
Carbon, C 0.18 %
0.18 %
Iron, Fe 98 %
98 %
As remainder
Manganese, Mn 1.6 %
1.6 %
Phosphorous, P 0.015 %
0.015 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0020 %
0.0020 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved