SMAC CABLE® 25235-10-08 Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name CABLE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC CABLE® 25235-10-08 Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloy Screws: Inox A2Threaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 110 daN
35.0 mm, 45° down and out
1290 daN
21.3 mm, down
3375 daN
15.0 mm, up
430.0 daN
18.0 mm, left and right
665.0 daN
18.0 mm, up and down
F, Max Static 250.0 daN
6.0 mm, up and down
250.0 daN
9.0 mm, left and right
450.0 daN
7.5 mm, 45° down and out
500.0 daN
5.8 mm, down
500.0 daN
2.5 mm, up
Transmissibility at resonance 3