Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloyClips: Stainless steelThreaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 19.0 daN
25.3 mm, 45° down and out
29.5 daN
15.5 mm, down
40.0 daN
18.5 mm, up and down
41.8 daN
20.2 mm, left and right
42.3 daN
6.3 mm, up
F, Max Static 10.0 daN
2.5 mm, down
10.0 daN
1.8 mm, up
5.0 daN
4.5 mm, up and down
5.0 daN
4.8 mm, left and right
7.5 daN
3.8 mm, 45° down and out
Transmissibility at resonance 3